Piranha Organic Aluminium_Oxide BreastCancerCell Anneal Global_Comm FM_SKPM STM HighAspect VinylAlcohol BCZT FastScan cooling Tin disulfide kelvin probe force microscopy Ca10(PO4)6(OH)2 Ceramics Fujian Wang FailureAnalysis 3-hexylthiophene HDD TemperatureControl Polytetrafluoroethylene self-assembly Metal Potential Formamidinium_lead_iodide molecule domain_switching DIWafer SmalScan PinpointNanomechanicalMode Lateral_Force_Microscopy ForceMapping
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Al2O3-doped CaMnO3
1% Al2O3-doped CaMnO3 on LaAlO3 (001) orientation substrate by pulsed laser deposition.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256