Laser TemperatureControl molecular_self_assembly Tapping 3-hexylthiophene Cross-section AdhesionForce MagneticForceMicroscopy Polyaniline TyphimuriumBiofilm KevlarFiber DLaTGS hetero_structure Vanadate Friction ForceVolumeImage Vortex Steps FrequencyModulation Ram Logo Aluminum temp_control Dopped LateralPFM BismuthVanadate NUS_Physics Corrosion ConductiveAFM CopperFoil Magnets LiNbO3 SICM Varistor IndiumTinOxide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Co coated surface
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.7Hz
- Pixel: 512×256
- Lift height: 30nm
- Scan Mode: MFM