fe_nd_b ferromagnetic PhthalocyaninePraseodymium 3-hexylthiophene PS_LDPE Hydroxyapatite Electronics Filter Polyvinylidene_fluoride InorganicCompound Logo vertical_PFM MagneticForce Workfunction CuFoil IRDetector CuSubstrate AmplitudeModulation Polystyrene Cobalt-dopedIronOxide amplitude_modulation Oxidation Pore Device Temasek_Lab MLCC BlockCopolymer Ferrite CHRYSALIS_INC AtomicLayer Potential Mobile AM_SKPM Spain SPMLabs
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Anodized Aluminum Oxide (AAO)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS
- Scan Size: 0.5Hz, 1Hz
- Scan Rate:20μm×20μm, 5μm×5μm
- Pixel: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AC160TS
- Scan Size: 0.5Hz, 1Hz
- Scan Rate:20μm×20μm, 5μm×5μm
- Pixel: 256 × 256