EvatecAG ThermalProperties Bmp Phosphide Ecoli Optoelectronic Current polymeric_arrays TungstenThinFilmDeposition Hair Resistance SrTiO3 fe_nd_b Fet Kevlar AmplitudeModulation Insulator MfmAmplitude TriGlycineSulphate University_of_Regensburg HighAcpectRatio flakes SKPM MetalCompound HexagonalBN align CuFoil TiO2 Ni81Fe19 LateralPFM atomic_steps Ferrite Wafer Scratch Friction
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256